METHOD FOR DIRECTLY PREPARING NICKEL SULFATE FROM LOW NICKEL MATTE, NICKEL SULFATE AND APPLICATION THEREOF

DRIVE February 8, 2024
Source
The present invention provides a method for directly preparing nickel sulfate from low nickel matte, a nickel sulfate and an application thereof, the method comprising the following steps: a) pre-treating a low nickel matte to obtain ferronickel powder; b) mixing the ferronickel powder with a sulfuric acid solution, stirring, dissolving, and then evaporating, to obtain a supersaturated sulfate solution; c) cooling the supersaturated sulfate solution to −5° C.-0° C., and performing suction filtration to obtain an insoluble solid; d) washing the insoluble solid with water, and removing impurities from the filtrate to obtain a nickel hydroxide precipitate; impurity removal comprising successively removing iron, and removing calcium and magnesium; e) washing the nickel hydroxide precipitate with water, acid-dissolving and evaporating to obtain nickel sulfate. The present invention increases the amount of nickel recovered, the purity of nickel sulfate being 18.10%-19.24% nickel, and the recovery rate being 94.8%-97.1%.

Discussion in the ATmosphere

Loading comments...