  "description": "A method is described to prepare a cathode material for high energy density rechargeable lithium ion batteries based on H 2 V 3 O 8 with improved cycling stability by means of a surface modification produced at low temperature in aqueous media. The battery comprises a stack composed by an anode, an…",
  "path": "/patents/969267",
  "publishedAt": "2014-10-01T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01D15/02",
    "BELENOS CLEAN POWER HOLDING AG [CH]"
  ],
  "textContent": "A method is described to prepare a cathode material for high energy density rechargeable lithium ion batteries based on H 2 V 3 O 8 with improved cycling stability by means of a surface modification produced at low temperature in aqueous media. The battery comprises a stack composed by an anode, an electrolytic layer, a separator and a cathode, whose material is based on a mixture of carbon black Li x H 2-x V 3 O 8 modified by an aluminum hydroxide coating achieved in a one pot multistep reaction using aluminum in an amount comprised between 0.5 wt% and 10 wt%.",
  "title": "Surface modified lithiated H2V3O8"
}