"$type": "site.standard.document",
"description": "A thermally sprayed coating (5) is formed on an inner surface of a cylinder bore (3) of a cylinder block (1) by using a thermal spray gun (7). The thermal spray gun (7) is reciprocated along an axial direction in the cylinder bore (3) while being rotated, and injects melted droplets (10) generated…",
"path": "/patents/969430",
"publishedAt": "2014-10-01T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C23C4/12",
"NISSAN MOTOR [JP]"
],
"textContent": "A thermally sprayed coating (5) is formed on an inner surface of a cylinder bore (3) of a cylinder block (1) by using a thermal spray gun (7). The thermal spray gun (7) is reciprocated along an axial direction in the cylinder bore (3) while being rotated, and injects melted droplets (10) generated by melting a wire made of a ferrous material from a nozzle (9) at its end. At this time, a moving speed of the thermal spray gun (7) along the axial direction into the cylinder bore (3) is made equal-to or larger-than a predetermined value, and the number of reciprocating cycles of the thermal spray gun (7) along the axial direction into the cylinder bore (3) is made equal-to or larger-than a predetermined value.",
"title": "MANUFACTURING METHOD FOR CYLINDER BLOCK"
}