  "description": "A battery electrode is obtained by a method comprising: mixing active material (A), carbon fibers (B) having a fiber diameter of not less than 50 nm and not more than 300 nm, carbon fibers (C) having a fiber diameter of not less than 5 nm and not more than 40 nm, carbon black (D) and a binder (E)…",
  "path": "/patents/970850",
  "publishedAt": "2014-08-27T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0525",
    "SHOWA DENKO KK [JP]"
  ],
  "textContent": "A battery electrode is obtained by a method comprising: mixing active material (A), carbon fibers (B) having a fiber diameter of not less than 50 nm and not more than 300 nm, carbon fibers (C) having a fiber diameter of not less than 5 nm and not more than 40 nm, carbon black (D) and a binder (E) by dry process to obtain a mixture; to the mixture, adding not less than 5/95 and not more than 20/80 of a liquid medium by mass relative to the total mass of the active material (A), the carbon fibers (B), the carbon fibers (C), carbon black (D) and the binder (E); performing kneading while applying shear stress; and shaping the kneaded material into a sheet form.",
  "title": "Method of manufacturing battery electrode"
}