  "$type": "site.standard.document",
  "description": "Disclosed is an austenitic stainless steel alloy that includes, by weight, about 16% to about 21% chromium, about 4.5% to about 5.5% nickel, about 2% to about 5% manganese, about 1% to about 2% silicon, about 0.8% to about 1.2% tungsten, about 0.4% to about 0.8% molybdenum, about 0.4% to about 0.6%…",
  "path": "/patents/971318",
  "publishedAt": "2014-08-13T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C22C38/02",
    "HONEYWELL INT INC [US]"
  ],
  "textContent": "Disclosed is an austenitic stainless steel alloy that includes, by weight, about 16% to about 21% chromium, about 4.5% to about 5.5% nickel, about 2% to about 5% manganese, about 1% to about 2% silicon, about 0.8% to about 1.2% tungsten, about 0.4% to about 0.8% molybdenum, about 0.4% to about 0.6% niobium, about 0.4% to about 0.5% carbon, and a balance of iron. The alloy is suitable for use in turbocharger turbine housing applications for temperature up to about 1020°C.",
  "title": "Stainless steel alloys, turbocharger turbine housings formed from the stainless steel alloys, and methods for manufacturing the same"
}