"description": "Disclosed are a method for manufacturing a secondary battery pouch film having at least an outer layer, a metal layer, a primer layer, and a sealant layer, or at least an outer layer, a metal layer, a primer layer, a melt-extrusion resin layer, and a sealant layer in this order, the method…",
"path": "/patents/1360407",
"publishedAt": "2024-03-07T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M50/183",
"Youlchon Chemical Co., Ltd."
],
"textContent": "Disclosed are a method for manufacturing a secondary battery pouch film having at least an outer layer, a metal layer, a primer layer, and a sealant layer, or at least an outer layer, a metal layer, a primer layer, a melt-extrusion resin layer, and a sealant layer in this order, the method including: a drying process of applying and heating a primer layer composition on the metal layer so as to dry the primer layer composition and cure at least a part of the primer layer composition. The organic solvent-based emulsion composition contains acid-modified polypropylene and a curing agent and has a curing start temperature of 150° C. or lower, preferably 135° C. to 150° C., and a drying process temperature of 150° C. or lower, preferably 135° C. to 150° C. The method is not subjected to a thermal lamination process when laminating sealant layer.",
"title": "PRIMER LAYER COMPOSITION, SECONDARY BATTERY POUCH FILM USING THE SAME, AND METHOD OF MANUFACTURING THE SAME"
}