"description": "A solid electrolyte represented by general formula LiSiR(MO), where x is an integer from 1 to 3 inclusive, y=4−x, each R present is independently C1-C3 alkyl or C1-C3 alkoxy, and M is sulfur, selenium, or tellurium. Methods of making the solid electrolyte include combining a phenylsilane and a…",
"path": "/patents/1362093",
"publishedAt": "2024-04-11T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/0564",
"Charles Austen ANGELL"
],
"textContent": "A solid electrolyte represented by general formula LiSiR(MO), where x is an integer from 1 to 3 inclusive, y=4−x, each R present is independently C1-C3 alkyl or C1-C3 alkoxy, and M is sulfur, selenium, or tellurium. Methods of making the solid electrolyte include combining a phenylsilane and a first acid to yield mixture including benzene and a second acid, and combining at least one of an alkali halide, and alkali amide, and an alkali alkoxide with the second acid to yield a product d represented by general formula LiSiR(MO). The second acid may be in the form of a liquid or a solid. The phenylsilane includes at least one C1-C3 alkyl substituent or at least one C1-C3 alkoxy substituent, and the first acid includes at least one of sulfuric acid, selenic acid, and telluric acid.",
"title": "Alkali ION Conducting Plastic Crystals"
}