POSITIVE ELECTRODE ACTIVE MATERIAL AND METHOD OF PRODUCING POSITIVE ELECTRODE ACTIVE MATERIAL

DRIVE May 9, 2024
Source
A method of producing a positive electrode active material, the method includes: contacting first particles that contain a lithium transition metal composite oxide with a solution containing sodium ions to obtain second particles containing the lithium transition metal composite oxide and sodium element, wherein the lithium transition metal composite oxide has a layered structure and a composition ratio of a number of moles of nickel to a total number of moles of metals other than lithium in a range of from 0.7 to less than 1; mixing the second particles and a boron compound to obtain a mixture; and heat-treating the mixture at a temperature in a range of from 100° C. to 450° C.