"description": "Disclosed in the present invention is a recovery process for a waste battery electrode sheet, the method comprising the following steps: subjecting a waste battery electrode sheet to shearing, drying and cold treatment, and then rolling and screening same to obtain a first positive electrode…",
"path": "/patents/1365308",
"publishedAt": "2024-06-20T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/54",
"GUANGDONG BRUNP RECYCLING TECHNOLOGY CO., LTD."
],
"textContent": "Disclosed in the present invention is a recovery process for a waste battery electrode sheet, the method comprising the following steps: subjecting a waste battery electrode sheet to shearing, drying and cold treatment, and then rolling and screening same to obtain a first positive electrode material and a first waste electrode sheet; subjecting the first waste electrode sheet to shearing, drying and cold treatment, and then rolling and screening same to obtain a second positive electrode material and a second waste electrode sheet; and roasting the first positive electrode material and the second positive electrode material to obtain a positive electrode powder. In the present invention, the aluminum content in the positive electrode material is reduced by means of step-by-step shearing, and the adhesion performance of a waste positive electrode plate binder is then reduced by means of vacuum freeze-drying and spraying with a quick-cooling agent. The aluminum foil of the positive electrode material does not easily break when being broken after vacuum freeze-drying, and the morphology and output of the aluminum foil after primary shearing and secondary shearing are basically unchanged.",
"title": "PICKLING-FREE RECOVERY PROCESS OF BATTERY ELECTRODE SHEET"
}