"$type": "site.standard.document",
"description": "A method for preparing a copper-based anode material from a waste battery includes the following steps: (1) disassembling a waste battery and taking out an anode plate; (2) using the anode plate in step (1) as an anode and taking a copper foil current collector as a cathode, and placing the anodeā¦",
"path": "/patents/1365980",
"publishedAt": "2024-07-04T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M10/54",
"GUANGDONG BRUNP RECYCLING TECHNOLOGY CO., LTD."
],
"textContent": "A method for preparing a copper-based anode material from a waste battery includes the following steps: (1) disassembling a waste battery and taking out an anode plate; (2) using the anode plate in step (1) as an anode and taking a copper foil current collector as a cathode, and placing the anode and the cathode in an electroplating solution for electroplating; (3) after the electroplating is completed, collecting anode powder separated from the anode and soaking the copper foil current collector in an acid solution; (4) washing and drying the soaked copper foil current collector; and (5) calcinating the copper foil current collector to obtain a copper-base anode material.",
"title": "METHOD FOR PREPARING COPPER-BASED NEGATIVE ELECTRODE MATERIAL BY USING WASTE BATTERY"
}