  "$type": "site.standard.document",
  "description": "A manufacturing method of a carbon-coated lithium iron phosphate material including steps of: (a) providing a first slurry, a lithium source, and a first carbon source having a first weight, wherein the first slurry is formed from an iron source and a phosphorus source, and the first weight is…",
  "path": "/patents/1366570",
  "publishedAt": "2024-07-11T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/366",
    "Advanced Lithium Electrochemistry Co., Ltd."
  ],
  "textContent": "A manufacturing method of a carbon-coated lithium iron phosphate material including steps of: (a) providing a first slurry, a lithium source, and a first carbon source having a first weight, wherein the first slurry is formed from an iron source and a phosphorus source, and the first weight is equal to an input value; (b) mixing and grinding the first carbon source, the lithium source and the first slurry to form a second slurry; (c) performing a carbon content analysis on the second slurry to obtain a loss value, wherein the loss value is smaller than the input value and greater than zero; (d) adding a second carbon source having a second weight into the second slurry to form a third slurry, wherein the second weight is equal to the loss value; (e) drying and sintering the third slurry to form the carbon-coated lithium iron phosphate material.",
  "title": "MANUFACTURING METHOD OF CARBON-COATED LITHIUM IRON PHOSPHATE MATERIAL"
}