  "$type": "site.standard.document",
  "description": "A polyethylene powder having a viscosity-average molecular weight of 200,000 or more and 10,000,000 or less, wherein complex viscosity under predetermined conditions for measurement of slurry viscoelasticity satisfies the following formula (1): −× 10≤ (|η*|(T): an absolute value of complex…",
  "path": "/patents/1366978",
  "publishedAt": "2024-07-18T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C08F10/02",
    "Asahi Kasei Kabushiki Kaisha"
  ],
  "textContent": "A polyethylene powder having a viscosity-average molecular weight of 200,000 or more and 10,000,000 or less, wherein complex viscosity under predetermined conditions for measurement of slurry viscoelasticity satisfies the following formula (1): −× 10≤ (|η*|(T): an absolute value of complex viscosity (Pas) at T, (T): an absolute value of complex viscosity (Pas) at T, T: maximum temperature (° C.) within a range in which the formula (2) is satisfied, T: minimum temperature (° C.) within a range in which the formula (2)) is satisfied: d(log|η*|)/dT ≤− () (|η*|: an absolute value of complex viscosity (Pas), T: temperature).",
  "title": "Polyethylene Powder, and Molded Body Thereof"
}