"description": "The present invention relates to a positive electrode active material for a lithium secondary battery having improved thermal stability, a method for producing the positive electrode active material, and a lithium secondary battery containing the same. The positive electrode active material may be…",
"path": "/patents/988703",
"publishedAt": "2013-07-17T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C01B25/45",
"SK INNOVATION CO LTD [KR]"
],
"textContent": "The present invention relates to a positive electrode active material for a lithium secondary battery having improved thermal stability, a method for producing the positive electrode active material, and a lithium secondary battery containing the same. The positive electrode active material may be represented by the following Chemical Formula 1 and contain particles having an average particle size of 200nm to 1 µ m, wherein the surfaces of the particles are coated with a uniform carbon coating layer. [Chemical Formula 1]Li a Mn 1-x M x PO 4 (Where, M is any one or a mixture of two or more selected from Mg, Fe, Co, Cr, Ti, Ni, Cu, Zn, Zr, Nb, and Mo, and a and x satisfy the following Equations: 0.9¤a¤1.1 and 0¤x",
"title": "POSITIVE ELECTRODE ACTIVE MATERIAL FOR A LITHIUM SECONDARY BATTERY, METHOD FOR PRODUCING SAME, AND LITHIUM SECONDARY BATTERY COMPRISING SAME"
}