"description": "Provided is a method for preparing a positive electrode active material for a lithium secondary battery, the method comprising: mixing and reacting a nickel source, a cobalt source, and an aluminum source, ammonia water, sucrose, and a pH adjusting agent to prepare a mixed solution; drying and…",
"path": "/patents/988705",
"publishedAt": "2013-07-17T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C01G53/10",
"SK INNOVATION CO LTD [KR]"
],
"textContent": "Provided is a method for preparing a positive electrode active material for a lithium secondary battery, the method comprising: mixing and reacting a nickel source, a cobalt source, and an aluminum source, ammonia water, sucrose, and a pH adjusting agent to prepare a mixed solution; drying and oxidizing the mixed solution to prepare a positive electrode active material precursor; and adding a lithium source to the positive electrode active material precursor and firing them to prepare a positive electrode active material for a lithium secondary battery.",
"title": "POSITIVE ELECTRODE ACTIVE MATERIAL FOR A LITHIUM SECONDARY BATTERY, AND METHOD FOR PREPARING SAME"
}