  "description": "A method for manufacturing cathode active material includes providing a polycrystalline transition metal precursor; providing a lithium salt composition including a first lithium salt and a second lithium salt having a eutectic melting temperature; creating a first mixture including the…",
  "path": "/patents/1375960",
  "publishedAt": "2025-06-19T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C30B1/12",
    "GM Global Technology Operations LLC"
  ],
  "textContent": "A method for manufacturing cathode active material includes providing a polycrystalline transition metal precursor; providing a lithium salt composition including a first lithium salt and a second lithium salt having a eutectic melting temperature; creating a first mixture including the polycrystalline transition metal precursor and the lithium salt composition; mixing the first mixture in a mixer to generate inter-frictional force to heat the lithium salt composition above the eutectic melting temperature and to generate a second mixture; and sintering the second mixture to form a spinel-coated single-crystal cathode active material.",
  "title": "PROCESS FOR SYTHESIZING SPINEL-COATED SINGLE-CRYSTAL CATHODE ACTIVE MATERIALS"
}