  "description": "A single-crystal cathode material and preparing method thereof are provided. The method involves mixing and ball milling a lithium source with a nickel-cobalt-manganese precursor and then performing a first sintering treatment to obtain the first main material. The first sintering temperature is…",
  "path": "/patents/1377294",
  "publishedAt": "2025-12-11T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C30B1/02",
    "GUIZHOU ZHENHUA E-CHEM INC."
  ],
  "textContent": "A single-crystal cathode material and preparing method thereof are provided. The method involves mixing and ball milling a lithium source with a nickel-cobalt-manganese precursor and then performing a first sintering treatment to obtain the first main material. The first sintering temperature is 650 to 950° C. and sintering time is 15 to 30 hours. The first main material is then mixed and ball-milled with source A and performing a second sintering treatment to prepare the single-crystal cathode material. The second sintering temperature is 650-950° C. and sintering time is 5-15 hours. A precursor is used to directly prepare a single-crystal cathode material without jet milling.",
  "title": "SINGLE-CRYSTAL CATHODE MATERIAL AND PREPARING METHOD THEREOF"
}