"description": "A production method of a roughly shaped material for an engine piston includes a continuous casting step for obtaining a cast rod (31) having a diameter of 85 mm or less by continuously casting a molten aluminum alloy (30) at a molten alloy temperature of 720 °C or higher, and a forging step for…",
"path": "/patents/1002450",
"publishedAt": "2012-05-16T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B21J1/04",
"SHOWA DENKO KK [JP]"
],
"textContent": "A production method of a roughly shaped material for an engine piston includes a continuous casting step for obtaining a cast rod (31) having a diameter of 85 mm or less by continuously casting a molten aluminum alloy (30) at a molten alloy temperature of 720 °C or higher, and a forging step for obtaining a roughly shaped material (11) for an engine piston by forging a forging material (32) obtained by homogenizing the cast bar (31) at 370 to 500 °C. A composition of the molten alloy (30) includes Si: 11.0 to 13.0 mass%, Fe: 0.6 to 1.0 mass%, Cu: 3.5 to 4.5 mass%, Mn: 0.25 mass% or less; Mg: 0.4 to 0.6 mass%, Cr: 0.15 mass% or less, Zr: 0.07 to 0.15 mass%, P: 0.005 to 0.010 mass%, Ca: 0.002 mass% or less, and the balance being Aluminum and inevitable impurities.",
"title": "PROCESS FOR PRODUCTION OF ROUGHLY SHAPED MATERIAL FOR ENGINE PISTON"
}