"$type": "site.standard.document",
"description": "A cushion gum of having a diene rubber and between 5 and 60 phr of a plasticizing hydrocarbon resin having a glass transition temperature greater than about 20°C, 60°C or even greater than 70°C and a number average molecular weight less than 2000. The cushion gum may comprise between 10 and 30 phr…",
"path": "/patents/1002462",
"publishedAt": "2012-05-16T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B29C73/02",
"MICHELIN SOC TECH [FR]"
],
"textContent": "A cushion gum of having a diene rubber and between 5 and 60 phr of a plasticizing hydrocarbon resin having a glass transition temperature greater than about 20°C, 60°C or even greater than 70°C and a number average molecular weight less than 2000. The cushion gum may comprise between 10 and 30 phr of the resin in particular embodiments. The plasticizing resin may be a terpene resin comprising units resulting from the polymerization of limonene, alpha pinene, beta pinene or combinations thereof; homopolymers or copolymers of cyclopentadiene (CPD) or dicyclopentadiene (DCPD), homopolymers or copolymers of terpene, homopolymers or copolymers of a C 5 cut and mixtures thereof; and/or copolymers of (D)CPD/ vinyl-aromatic, of (D)CPD/ terpene, of (D)CPD/ C 5 cut, of teipene/vinyl-aromatic, of C 5 cut/vinyl-aromatic and of combinations thereof.",
"title": "Rubber retreading formulation"
}