  "$type": "site.standard.document",
  "description": "The present disclosure provides a method for preparing a porous micron-sized silicon ball negative electrode material, including the following steps: performing high-temperature expansion and mechanical ball milling on a layered silicate raw material, and purifying same by hydrochloric acid washing…",
  "path": "/patents/1378792",
  "publishedAt": "2026-02-26T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01B33/023",
    "WUHAN UNIVERSITY OF SCIENCE AND TECHNOLOGY"
  ],
  "textContent": "The present disclosure provides a method for preparing a porous micron-sized silicon ball negative electrode material, including the following steps: performing high-temperature expansion and mechanical ball milling on a layered silicate raw material, and purifying same by hydrochloric acid washing to obtain a layered silicon dioxide; mixing the layered silicon dioxide with aluminum powder, sodium chloride and aluminum chloride, putting the mixture into a reaction container, and heating the mixture to perform a reduction reaction; and washing the reaction product by using a hydrochloric acid and hydrofluoric acid solution, then performing suction filtration to be neutral, and vacuum-drying same to obtain the porous micron-sized silicon ball.",
  "title": "POROUS MICRON-SIZED SILICON BALL MATERIAL AND PREPARATION METHOD THEREFOR AND USE THEREOF"
}