"$type": "site.standard.document",
"coverImage": {
"$type": "blob",
"ref": {
"$link": "bafkreigfrk6clr6lwbystxk4jr2yjzqbqao7ymjx23rdvtpuifqfqpnthu"
},
"mimeType": "image/png",
"size": 87146
},
"description": "The present invention provides a non-aqueous electrolyte-based high power lithium secondary battery having a long-term service life and superior safety at both room temperature and high temperature, even after repeated high-current charging and discharging, wherein the battery comprises a mixture…",
"path": "/patents/1007066",
"publishedAt": "2011-12-21T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C01G45/1242",
"LG CHEMICAL LTD [KR]"
],
"textContent": "The present invention provides a non-aqueous electrolyte-based high power lithium secondary battery having a long-term service life and superior safety at both room temperature and high temperature, even after repeated high-current charging and discharging, wherein the battery comprises a mixture of a particular lithium manganese-metal composite oxide (A) having a spinel structure and a particular lithium nickel-manganese-cobalt composite oxide (B) having a layered structure, as a cathode active material.",
"title": "Method for fabricating a cathode"
}