  "description": "A positive active material for a rechargeable lithium battery includes pores having an average diameter of about 10 nm to about 60 nm and a porosity of about 0.5 % to about 20 %. Also disclosed is a method of preparing the positive active material, a rechargeable lithium battery including the…",
  "path": "/patents/1007089",
  "publishedAt": "2011-12-14T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/505",
    "SAMSUNG SDI CO LTD [KR]"
  ],
  "textContent": "A positive active material for a rechargeable lithium battery includes pores having an average diameter of about 10 nm to about 60 nm and a porosity of about 0.5 % to about 20 %. Also disclosed is a method of preparing the positive active material, a rechargeable lithium battery including the positive active material, and use of the positive active material in a rechargeable lithium battery.",
  "title": "Positive active material for rechargeable lithium battery, method of preparing the same, and rechargeable lithium battery including the same"
}