  "$type": "site.standard.document",
  "description": "A method for producing a sulfide solid electrolyte including an argyrodite-type crystal structure includes: pulverizing and mixing raw materials with a pulverizer to prepare an intermediate containing a glass component, wherein the raw materials include lithium, phosphorus, sulfur, and chlorine…",
  "path": "/patents/1380535",
  "publishedAt": "2026-04-02T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0562",
    "IDEMITSU KOSAN CO., LTD."
  ],
  "textContent": "A method for producing a sulfide solid electrolyte including an argyrodite-type crystal structure includes: pulverizing and mixing raw materials with a pulverizer to prepare an intermediate containing a glass component, wherein the raw materials include lithium, phosphorus, sulfur, and chlorine; and heat-treating the intermediate at 360 to 500° C. A molar ratio of the chlorine to the phosphorus, c (CIP), of the raw materials is greater than 1.0 and 1.9 or less.",
  "title": "SULFIDE SOLID ELECTROLYTE"
}