  "$type": "site.standard.document",
  "description": "Sulfur-crosslinkable rubber mixture (I) comprises: at least a functionalized diene rubber, whose functionalization is present along the polymer chain and/or at the end and enables for binding at fillers, where the diene rubber has a glass transition temperature of -110 to -15[deg] C; at least an…",
  "path": "/patents/1010065",
  "publishedAt": "2011-08-17T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B29B7/7495",
    "CONTINENTAL REIFEN DEUTSCHLAND [DE]"
  ],
  "textContent": "Sulfur-crosslinkable rubber mixture (I) comprises: at least a functionalized diene rubber, whose functionalization is present along the polymer chain and/or at the end and enables for binding at fillers, where the diene rubber has a glass transition temperature of -110 to -15[deg] C; at least an aliphatic and/or aromatic hydrocarbon resin with a softening point (ring and ball according to ASTM E 28) of 50-150[deg] C and a number average molecular weight of 200-2000 g/mole and a polydispersity of 15; and at least a filler.",
  "title": "SULPHUR CROSSLINKABLE RUBBER COMPOSITION"
}