  "$type": "site.standard.document",
  "description": "A method for manufacturing LMFP composite positive electrode particles includes the steps of: placing a plurality of lithium ion conductor particles and LMFP particles, a carbon source and a first dispersant into a ball mill for mixing to form a mixed slurry, wherein each of the lithium ion…",
  "path": "/patents/1382237",
  "publishedAt": "2026-05-07T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M4/0471",
    "ZHI FENG LUO"
  ],
  "textContent": "A method for manufacturing LMFP composite positive electrode particles includes the steps of: placing a plurality of lithium ion conductor particles and LMFP particles, a carbon source and a first dispersant into a ball mill for mixing to form a mixed slurry, wherein each of the lithium ion conductor particles formed by a first oxide or phosphate capable of conducting lithium ions, or is formed by a second oxide with a garnet structure or a perovskite structure; then performing a drying on the mixed slurry to obtain a plurality of mixture powders; and then placing the mixture powders into a sintering furnace for performing an oxygen-free sintering to cause that the carbon source performs a dehydration reaction to produce carbons and other residues to form a conductive layer coated on the outer surface of each of the LMFP particles.",
  "title": "METHOD FOR MANUFACTURING LMFP COMPOSITE POSITIVE ELECTRODE PARTICLES"
}