  "description": "A solid electrolyte material comprises Li, T, X and A wherein T is at least one of P, As, Si, Ge, Al, and B; X is one or more halogens or N; A is one or more of S and Se. The solid electrolyte material has peaks at 17.8°±0.75° and 19.2°±0.75° in X-ray diffraction measurement with Cu-Kα(1,2)=1.5418…",
  "path": "/patents/1382732",
  "publishedAt": "2026-05-14T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0562",
    "Solid Power Operating, Inc."
  ],
  "textContent": "A solid electrolyte material comprises Li, T, X and A wherein T is at least one of P, As, Si, Ge, Al, and B; X is one or more halogens or N; A is one or more of S and Se. The solid electrolyte material has peaks at 17.8°±0.75° and 19.2°±0.75° in X-ray diffraction measurement with Cu-Kα(1,2)=1.5418 Å and may include glass ceramic and/or mixed crystalline phases.",
  "title": "SOLID ELECTROLYTE MATERIAL AND SOLID-STATE BATTERY MADE THEREWITH"
}