"description": "A method of producing a nickel-cobalt composite hydroxide includes: preparing a first solution containing nickel ions and cobalt ions; preparing a second solution containing tungsten ions and having a pH of 10 or more; preparing a third solution containing a complex ion-forming factor; preparing a…",
"path": "/patents/1384995",
"publishedAt": "2017-11-09T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M4/525",
"NICHIA CORPORATION"
],
"textContent": "A method of producing a nickel-cobalt composite hydroxide includes: preparing a first solution containing nickel ions and cobalt ions; preparing a second solution containing tungsten ions and having a pH of 10 or more; preparing a third solution containing a complex ion-forming factor; preparing a liquid medium having a pH in a range of 10 to 13.5; supplying the first solution, the second solution, and the third solution separately and simultaneously to the liquid medium to obtain a reacted solution having a pH in a range of 10 to 13.5; and obtaining the nickel-cobalt composite hydroxide containing nickel, cobalt, and tungsten from the reacted solution.",
"title": "METHOD OF PRODUCING NICKEL-COBALT COMPOSITE HYDROXIDE AND METHOD OF PRODUCING POSITIVE ELECTRODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY"
}