  "description": "Nickel oxyhydroxide can be prepared by exposing a mixture of a nickel hydroxide and a hydroxide salt to ozone. The nickel oxyhydroxide is suitable for use in the cathode of a battery.",
  "path": "/patents/1015414",
  "publishedAt": "2011-03-02T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C01G53/04",
    "GILLETTE CO [US]"
  ],
  "textContent": "Nickel oxyhydroxide can be prepared by exposing a mixture of a nickel hydroxide and a hydroxide salt to ozone. The nickel oxyhydroxide is suitable for use in the cathode of a battery.",
  "title": "Preparation of nickel oxyhydroxide using ozone"
}