"$type": "site.standard.document",
"description": "Each of at least two layers of a carcass reinforcement has a breaking force per unit width higher than 2250 daN/dm. The minimum strength per unit width, measured for an elongation of less than 10%, of a second layer of carcass reinforcement is strictly greater than a value equal to 20% of the…",
"path": "/patents/1385045",
"publishedAt": "2017-11-16T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B60C15/0054",
"COMPAGNIE GENERALE DES ETABLISSEMENTS MICHELIN"
],
"textContent": "Each of at least two layers of a carcass reinforcement has a breaking force per unit width higher than 2250 daN/dm. The minimum strength per unit width, measured for an elongation of less than 10%, of a second layer of carcass reinforcement is strictly greater than a value equal to 20% of the minimum strength per unit width, measured for an elongation of less than 10%, of a first layer of carcass reinforcement. The reinforcing elements of the two layers of carcass reinforcement have a thread count of less than 750 tex. The elongation of the reinforcing elements of the second layer of carcass reinforcement is greater than 4% under a force of 20 daN, and the secant elastic modulus values under tension at 10% elongation, Mt, Mj, satisfy the relationship Mt/Mj≧1.",
"title": "TIRE COMPRISING A CARCASS REINFORCEMENT MADE UP OF TWO LAYERS"
}