"$type": "site.standard.document",
"coverImage": {
"$type": "blob",
"ref": {
"$link": "bafkreiemkp7hrsd5m2jadsb6yixnvrqpks7wclwsfynt5ezf5cfezvagmy"
},
"mimeType": "image/png",
"size": 102872
},
"description": "A method for manufacturing an electrically-conductive paste includes: bringing carbon nanotubes (CNT) and a solvent into contact with each other so that a wetting rate is 25 to 125%; kneading, by using a planetary stirring machine, a mixture containing the CNT and the solvent obtained by…",
"path": "/patents/1357053",
"publishedAt": "2023-12-28T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01B1/04",
"SANYO COLOR WORKS, Ltd."
],
"textContent": "A method for manufacturing an electrically-conductive paste includes: bringing carbon nanotubes (CNT) and a solvent into contact with each other so that a wetting rate is 25 to 125%; kneading, by using a planetary stirring machine, a mixture containing the CNT and the solvent obtained by impregnating the CNT with the solvent, to obtain a kneaded product in a paste state; and then performing dispersion processing on a dilution obtained by mixing a solvent into the obtained kneaded product.",
"title": "METHOD FOR MANUFACTURING ELECTRICALLY-CONDUCTIVE PASTE"
}