"description": "A piston (1) has a piston body (10) made of a material selected from any one of aluminum, an aluminum alloy, magnesium, and a magnesium alloy containing 12-25% silicon. An entire surface or a predetermined portion of the surface of the piston body (10) is covered with a plasma oxide film (17) by a…",
"path": "/patents/1067387",
"publishedAt": "2006-05-17T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C25D11/026",
"AISIN SEIKI [JP]"
],
"textContent": "A piston (1) has a piston body (10) made of a material selected from any one of aluminum, an aluminum alloy, magnesium, and a magnesium alloy containing 12-25% silicon. An entire surface or a predetermined portion of the surface of the piston body (10) is covered with a plasma oxide film (17) by a microarc-oxidation process.",
"title": "Aluminium-piston containing 12-25% Silicon, the surface of which is oxidised by microarc-oxidation"
}