"$type": "site.standard.document",
"description": "The procedure for fixing a component weight 15-90 g, such as a pressure sensor, to the inner surface channel of a vehicle wheel (12) rim inside a pneumatic tyre (14) uses an adhesive with a tensile stress greater than 0.5 MPa at 80[deg]C, containing at least one polymer ingredient with a vitreous…",
"path": "/patents/1074573",
"publishedAt": "2005-08-31T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"B60C23/0408",
"MICHELIN SOC TECH [FR]"
],
"textContent": "The procedure for fixing a component weight 15-90 g, such as a pressure sensor, to the inner surface channel of a vehicle wheel (12) rim inside a pneumatic tyre (14) uses an adhesive with a tensile stress greater than 0.5 MPa at 80[deg]C, containing at least one polymer ingredient with a vitreous transition temperature below -50[deg]C and at least one other polymer ingredient with a vitreous transition temperature above 100[deg]C. The adhesive is allowed to set for a period of 45-55 s before the tyre is fitted to the wheel.",
"title": "Use of an adhesive to bond a device to a wheel, the device-wheel system, the device and the wheel"
}