"description": "In a power storage device, a welding portion at which a first conductive member and a second conductive member are welded is formed, an outer peripheral edge of a base portion includes a first portion located in a vicinity of the welding portion and a second portion other than the first portion…",
"path": "/patents/1114840",
"publishedAt": "2026-05-28T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"H01M50/536",
"Prime Planet Energy & Solutions, Inc."
],
"textContent": "In a power storage device, a welding portion at which a first conductive member and a second conductive member are welded is formed, an outer peripheral edge of a base portion includes a first portion located in a vicinity of the welding portion and a second portion other than the first portion, and the outer peripheral wall is not formed in the first portion, or a maximum value of a height of the outer peripheral wall in the first portion is lower than a maximum value of a height of an outer peripheral wall in the second portion.",
"title": "POWER STORAGE DEVICE AND METHOD OF MANUFACTURING SAME"
}