  "description": "Production of nanocrystalline lithium titanate spinels (I) involves reacting lithium hydroxide and titanium alcoholate (II) at elevated temperature in a reaction mixture forming water of reaction. An independent claim is included for nanocrystalline lithium titanate spinels (I) obtained by the…",
  "path": "/patents/1082646",
  "publishedAt": "2004-11-03T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B82Y30/00",
    "BASF AG [DE]"
  ],
  "textContent": "Production of nanocrystalline lithium titanate spinels (I) involves reacting lithium hydroxide and titanium alcoholate (II) at elevated temperature in a reaction mixture forming water of reaction. An independent claim is included for nanocrystalline lithium titanate spinels (I) obtained by the above process and having a particle size of 1-200 nm.",
  "title": "Process for preparing nanocrystalline lithium titanate spinels"
}