  "$type": "site.standard.document",
  "description": "A thermal spray coated piston ring having improved initial running-in propery, and having scuffing resistance and wear resistance is provided. The spray coating film (3) of the piston ring (1) contains from 2 to 40 mass % of Sn and from 5 to 50 mass % of graphite, and if necessary, P, Sb, Co, Be…",
  "path": "/patents/1083259",
  "publishedAt": "2004-10-13T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C23C4/02",
    "RIKEN KK [JP]"
  ],
  "textContent": "A thermal spray coated piston ring having improved initial running-in propery, and having scuffing resistance and wear resistance is provided. The spray coating film (3) of the piston ring (1) contains from 2 to 40 mass % of Sn and from 5 to 50 mass % of graphite, and if necessary, P, Sb, Co, Be, Cr, Mn, Si, Cd, Zn, Fe, Ni and/or Pb, the balance essentially consisting of Cu.",
  "title": "SPRAYING PISTON RING"
}