  "$type": "site.standard.document",
  "description": "Composition for solid polymer electrolyte contains a polyether polymer containing =5 weight% toluene insolubles, or a polyether of Mooney viscosity 3-190 formed by reducing the Mooney viscosity by >=5 by applying a shear force to a polyether polymer of Mooney viscosity 10-200 under heating using an…",
  "path": "/patents/1087546",
  "publishedAt": "2004-05-06T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "C08G65/14",
    "ZEON CORP [JP]"
  ],
  "textContent": "Composition for solid polymer electrolyte contains a polyether polymer containing =5 weight% toluene insolubles, or a polyether of Mooney viscosity 3-190 formed by reducing the Mooney viscosity by >=5 by applying a shear force to a polyether polymer of Mooney viscosity 10-200 under heating using an extruder, and an electrolyte salt compound soluble in the polymer. Independent claims are also included for the following: (1) the solid polymer electrolyte formed by crosslinking the composition; (2) the battery formed which has the polymer solid electrolyte; (3) the polyether polymer of Mooney viscosity 3-190 formed by reducing the Mooney viscosity by >=5 by applying a shear force to a polyether polymer of Mooney viscosity 10-200 under heating using an extruder; and (4) the manufacture of the polyether polymer of Mooney viscosity 3-190.",
  "title": "POLYETHER POLYMER, PROCESS FOR PRODUCING THE SAME, COMPOSITION FOR SOLID POLYMER ELECTROLYTE AND USE THEREOF"
}