  "$type": "site.standard.document",
  "description": "An elongated bumper core of a polyolefin-based resin-containing foam having a density of 0.045-0.2 g/cm 3 and showing a compressive load of F 20 at 20 % strain, a compressive load of F 40 at 40 % strain and a compressive load of F 60 at 60 % strain when compressed by a rigid pipe having an outer…",
  "path": "/patents/1089180",
  "publishedAt": "2004-03-03T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B60R19/18",
    "JSP CORP [JP]"
  ],
  "textContent": "An elongated bumper core of a polyolefin-based resin-containing foam having a density of 0.045-0.2 g/cm 3 and showing a compressive load of F 20 at 20 % strain, a compressive load of F 40 at 40 % strain and a compressive load of F 60 at 60 % strain when compressed by a rigid pipe having an outer diameter of 70 mm at a compression speed of 500 mm/minute, wherein the ratio F 20 /F 40 is in the range of 0.6-1.3 and the ratio F 60 /F 40 is in the range of 0.75-1.3.",
  "title": "Bumper core"
}