  "description": "A first manufacturing method of a totally solid polymer secondary battery includes laminating a first quasi-positive electrode layer (20a) on a positive electrode current collector (25), laminating a polymer solid electrolyte layer (10) and a second quasi-positive electrode layer (20b) on the…",
  "path": "/patents/1098499",
  "publishedAt": "2003-02-05T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/0525",
    "NISSAN MOTOR [JP]"
  ],
  "textContent": "A first manufacturing method of a totally solid polymer secondary battery includes laminating a first quasi-positive electrode layer (20a) on a positive electrode current collector (25), laminating a polymer solid electrolyte layer (10) and a second quasi-positive electrode layer (20b) on the negative electrode layer (30), and adhering the first and second quasi-positive electrode layers to each other. A second manufacturing method of the same includes laminating a positive electrode layer (20) and a first quasi-polymer solid electrolyte layer (10a) on a positive electrode current collector (25), laminating a negative electrode layer (30) and a second quasi-polymer solid electrolyte layer (10b) on a negative electrode current collector, and adhering the first and second quasi-polymer solid electrolyte layers to each other. A third manufacturing method of the same includes laminating a positive electrode layer (20), a polymer solid electrolyte layer (10) and a first quasi-negative electrode layer (30a) on a positive electrode current collector (25), forming a second quasi-negative electrode layer (30b) on a negative electrode current collector (35), and adhering the first and second quasi-negative electrode layers to each other.",
  "title": "Totally solid type polymer lithium ion secondary battery and manufacturing method of the same"
}