  "description": "A lead alloy coating (24) for a positive grid (20) of a lead acid battery (52) is provided. The lead alloy coating includes a tin content of at least about 0.1%, but not more than about 3%; and a residual lead content. The lead alloy coating optionally includes a calcium content of at least about…",
  "path": "/patents/1098835",
  "publishedAt": "2003-01-22T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B32B15/01",
    "DELPHI TECH INC [US]"
  ],
  "textContent": "A lead alloy coating (24) for a positive grid (20) of a lead acid battery (52) is provided. The lead alloy coating includes a tin content of at least about 0.1%, but not more than about 3%; and a residual lead content. The lead alloy coating optionally includes a calcium content of at least about 0.01%, but not more than about 0.1%, with or without a silver content of at least about 0.01%, but not more than about 0.1%. Alternatively, the lead alloy coating optionally includes a barium content of at least about 0.01%, but not more than about 0.1%, with or without a silver content of at least about 0.01%, but not more than about 0.1%.",
  "title": "Lead alloy surface coating for positive lead-acid battery grids and methods of use"
}