  "$type": "site.standard.document",
  "description": "The rubber-reinforcing fiber of the present invention is provided with a coating layer of a thickness of 10 ANGSTROM to 40 mu m. The coating layer is formed by dry plating and contains at least one metal and/or metal compound selected from the group consisting of cobalt, zinc, copper, titanium…",
  "path": "/patents/1098936",
  "publishedAt": "2003-01-22T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "B29B15/08",
    "BRIDGESTONE CORP [JP]"
  ],
  "textContent": "The rubber-reinforcing fiber of the present invention is provided with a coating layer of a thickness of 10 ANGSTROM to 40 mu m. The coating layer is formed by dry plating and contains at least one metal and/or metal compound selected from the group consisting of cobalt, zinc, copper, titanium, silver, nickel and compounds of the aforesaid metals. With such a coating layer, the rubber-reinforcing fiber of the present invention forms a firm adhesion to a rubber component and drastically improves the fatigue resistance and durability of a rubber article, particularly, a pneumatic tire.",
  "title": "RUBBER-REINFORCING FIBER, PROCESS FOR PRODUCING THE SAME, AND RUBBER PRODUCT AND PNEUMATIC TIRE EACH MADE WITH THE SAME"
}