Silver vanadium oxide having low internal resistance and method of manufacture

DRIVE July 3, 2002
Source
The current invention relates to the preparation of an improved cathode active material for non-aqueous lithium electrochemical cell. In particular, the cathode active material comprises ε-phase silver vanadium oxide prepared by using a γ-phase silver vanadium oxide starting material. The reaction of γ-phase SVO with a silver salt produces the novel ε-phase SVO possessing a lower surface area than ε-phase SVO produced from vanadium oxide (VO) and a similar silver salt as starting materials. Consequently, the low surface area ε-phase SVO material provides an advantage in greater long term stability in pulse dischargeable cells.