"$type": "site.standard.document",
"description": "A solid oxide fuel cell in which the catalytic activity of a fuel electrode is high and in which no poisoning by carbon occurs even when internal reforming is performed under a condition of a low S/C ratio and further in which the time course degradation of the fuel electrode is less when internal…",
"path": "/patents/1104743",
"publishedAt": "2002-05-02T00:00:00.000Z",
"site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
"tags": [
"C04B35/486",
"TOHO GAS KK [JP]"
],
"textContent": "A solid oxide fuel cell in which the catalytic activity of a fuel electrode is high and in which no poisoning by carbon occurs even when internal reforming is performed under a condition of a low S/C ratio and further in which the time course degradation of the fuel electrode is less when internal reforming is performed. In a solid oxide fuel cell having an oxide ion conductive solid electrolyte, and a fuel electrode and an air electrode connected to both faces thereof, a cermet of a catalyst and of the second solid electrolyte whose oxide ion conductivity is more than or equal to 0.2 S/cm at 1000 DEG C is used as the fuel electrode. More specifically, it is desirable that the second solid electrolyte is scandia-stabilized zirconia (ScSZ) containing 9 to 12 mol% of scandia.",
"title": "Solid oxide fuel cell"
}