  "description": "Anode material consists of coated metal cores made from antimony, bismuth, cadmium, indium, lead, gallium, tin or their alloys. Independent claims are also included for: (A) a process for the production of the anode material comprising producing a suspension or a sol of the metal or alloy core in…",
  "path": "/patents/1109605",
  "publishedAt": "2001-10-04T00:00:00.000Z",
  "site": "at://did:plc:oql6ds5vnff4ugar6rruliwd/site.standard.publication/3mn3ohu7oxx5w",
  "tags": [
    "H01M10/052",
    "MERCK PATENT GMBH [DE]"
  ],
  "textContent": "Anode material consists of coated metal cores made from antimony, bismuth, cadmium, indium, lead, gallium, tin or their alloys. Independent claims are also included for: (A) a process for the production of the anode material comprising producing a suspension or a sol of the metal or alloy core in urotropin; emulsifying the suspension with 5-12C hydrocarbons; precipitating the emulsion on the metal or alloy cores; and converting the metal hydroxide and/or oxyhydroxide into the corresponding oxide by tempering the system; and (B) an electrochemical cell consisting of a cathode, separator, electrolyte and the anode made of the above material.",
  "title": "Active material for anodes in electrochemical cells and process of manufacture thereof"
}